SAE AMS5841E-2006
Cobalt-Nickel Alloy, Corrosion and Heat Resistant, Bars 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb - 2.9Ti - 0.20Al - 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated for Work Strengthening UNS R30159

Standard No.
SAE AMS5841E-2006
Release Date
2006
Published By
Society of Automotive Engineers (SAE)
Status
Replace By
SAE AMS5841F-2011
Latest
SAE AMS5841G-2022
Scope
This specification covers a high strength, corrosion and heat resistant cobalt-chromium-nickel alloy in the form of bars. These bars have been used typically for applications requiring a combination of high strength up to 1100 degrees F (593 degrees C), good tension-tension fatigue strength, toughness, and ductility, but usage is not limited to such applications. This alloy exhibits exceptionally good resistance to corrosion, crevice-corrosion, stress-corrosion cracking, and elevated temperature relaxation.

SAE AMS5841E-2006 history

  • 2022 SAE AMS5841G-2022 Cobalt-Nickel Alloy, Corrosion and Heat-Resistant, Bars 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb (Nb) - 2.9Ti - 0.20Al - 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated for Work Strengthening
  • 2016 SAE AMS5841G-2016 Cobalt-Nickel Alloy@ Corrosion and Heat-Resistant@ Bars 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb (Nb) - 2.9Ti - 0.20Al - 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated for Work Strengthening (UNS R30159)
  • 2011 SAE AMS5841F-2011 Cobalt-Nickel Alloy, Corrosion and Heat Resistant, Bars 19Cr 36Co 25Ni 7.0Mo 0.50Cb (Nb) 2.9Ti 0.20Al 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated For Work Strengthening
  • 2006 SAE AMS5841E-2006 Cobalt-Nickel Alloy, Corrosion and Heat Resistant, Bars 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb - 2.9Ti - 0.20Al - 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated for Work Strengthening UNS R30159
  • 2000 SAE AMS5841D-2000 Cobalt-Nickel Alloy, Corrosion and Heat Resistant, Bars 19Cr 36Co 25Ni 7.0Mo 0.50Cb 2.9Ti 0.20Al 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated For Work Strengthening
  • 1994 SAE AMS5841C-1994 Alloy@ Corrosion and Heat Resistant@ Bars 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb - 2.9Ti - 0.20Al - 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated for Work Strengthening (UNS R30159)
  • 1989 SAE AMS5841B-1989 ALLOY BARS, CORROSION AND HEAT RESISTANT 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb - 2.9Ti - 0.20Al - 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated for Work Strengthening
  • 1983 SAE AMS5841A-1983 ALLOY BARS, CORROSION AND HEAT RESISTANT 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb - 2.9Ti - 0.20Al - 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated for Work Strengthening
  • 1977 SAE AMS5841-1977 ALLOY BARS, CORROSION AND HEAT RESISTANT 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb - 2.9Ti - 0.20Al - 9.0Fe Solution Heat Treated for Work Strengthening



Copyright ©2024 All Rights Reserved