Scope
This specification covers a corrosion and heat resistant nickel alloy in the form of forgings and forging stock. These forgings have been used typically for rotating parts, such as compressor blades, discs, hubs, shafts, and spacers requiring high strength up to 1500 degrees F (816 degrees C) and oxidation resistance up to 1750 degrees F (954 degrees C), but usage is not limited to such applications.

SAE AMS5704H-2006 history

  • 2020 SAE AMS5704L-2020 Nickel Alloy, Corrosion and Heat Resistant, Forgings 57Ni - 19.5Cr - 13.5Co - 4.6Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1825 to 1900 °F (996 to 1038 °C) Solution, Stabilization, and Precipitation Heat Treated
  • 2015 SAE AMS5704K-2015 Nickel Alloy@ Corrosion and Heat Resistant@ Forgings 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1825 to 1900 ��(996 to 1038 �� Solution@ Stabilization@ and Precipitation Heat Treated
  • 2013 SAE AMS5704J-2013 Nickel Alloy, Corrosion and Heat-Resistant, Forgings 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1825 to 1900 °F (996 to 1038 °C) Solution, Stabilization, and Precipitation Heat Treated
  • 2008 SAE AMS5704J-2008 Nickel Alloy, Corrosion and Heat Resistant, Forgings 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1825 to 1900 Degrees F (996 to 1038 Degrees C) Solution, Stabilization, and Precipitatio
  • 2006 SAE AMS5704H-2006 Nickel Alloy, Corrosion and Heat Resistant, Forgings 57Ni 19.5Cr 13.5Co 4.3Mo 3.0Ti 1.4Al 0.05Zr 0.006B, Consumable Electrode or Vacuum Induction Melted, 1825 to 1900°F (996 to 1038°C) Solution, Stabilization, and Precipitation Heat Treated
  • 2000 SAE AMS5704G-2000 Nickel Alloy, Corrosion and Heat Resistant, Forgings 57Ni 19.5Cr 13.5Co 4.3Mo 3.0Ti 1.4Al 0.05Zr 0.006B, Consumable Electrode or Vacuum Induction Melted, 1825 to 1900°F (996 to 1038°C) Solution, Stabilization, and Precipitation Heat Treated
  • 1995 SAE AMS5704F-1995 Nickel Alloy@ Corrosion and Heat Resistant@ Forgings 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1825 to 1900 Degrees F (996 to 1038 Degrees C) Solution@ Stabilization@ and Precipitation
  • 1993 SAE AMS5704E-1993 NICKEL ALLOY, CORROSION AND HEAT RESISTANT, FORGINGS 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1825 to 1900 °F (996 to 1038 °C) Solution, Stabilization, and Precipitation Heat Treated
  • 1988 SAE AMS5704D-1988 ALLOY FORGINGS, CORROSION AND HEAT RESISTANT 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1825° - 1900°F (995° - 1040°C) Solution, Stabilization, and Precipitation Heat Treated
  • 1982 SAE AMS5704C-1982 ALLOY FORGINGS, CORROSION AND HEAT RESISTANT 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1825° - 1900°F (995° - 1040°C) Solution, Stabilization, and Precipitation Heat Treated
  • 1976 SAE AMS5704B-1976 ALLOY FORGINGS, CORROSION AND HEAT RESISTANT 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1825° - 1900° F (996° - 1038° C) Solution, Stabilization, and Precipitation Heat Treated
  • 1970 SAE AMS5704A-1970 ALLOY FORGINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Consumable Electrode or Vacuum Induction Melted 1825 - 1900 F (996.1 - 1037.8 C) Solution, Stabilization, and Precipitation Heat Treated
  • 1966 SAE AMS5704-1966 ALLOY FORGINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al Solution, Stabilization, and Precipitation Heat Treated 1825 - 1900 F (996.1 - 1037.8 C) Treatment Consumable Electrode or Vacuum Induction Melted



Copyright ©2024 All Rights Reserved