SAE AMS4281F-2001
Aluminum Alloy Castings, Permanent Mold 5.0Si 1.2Cu 0.5Mg (355.0-T6) Solution and Precipitation Heat Treated

Standard No.
SAE AMS4281F-2001
Release Date
2001
Published By
Society of Automotive Engineers (SAE)
Status
Replace By
SAE AMS4281F-2006
Latest
SAE AMS4281G-2014
Scope
This specification covers an aluminum alloy in the form of permanent mold castings. These castings have been used typically for parts requiring moderate strength at temperatures up to 300 degrees F (149 degrees C), but usage is not limited to such applications.

SAE AMS4281F-2001 history

  • 2014 SAE AMS4281G-2014 Aluminum Alloy Castings, Permanent Mold 5.0Si - 1.2Cu - 0.50Mg (355.0-T6) Solution and Precipitation Heat Treated
  • 2008 SAE AMS4281G-2008 Aluminum Alloy Castings, Permanent Mold 5.0Si 1.2Cu 0.5Mg (355.0-T6) Solution and Precipitation Heat Treated
  • 2006 SAE AMS4281F-2006 Aluminum Alloy Castings, Permanent Mold 5.0Si - 1.2Cu - 0.50Mg (355.0-T6) Solution and Precipitation Heat Treated
  • 2001 SAE AMS4281F-2001 Aluminum Alloy Castings, Permanent Mold 5.0Si 1.2Cu 0.5Mg (355.0-T6) Solution and Precipitation Heat Treated
  • 1994 SAE AMS4281E-1994 ALUMINUM ALLOY CASTINGS, PERMANENT MOLD 5.0Si - 1.2Cu - 0.50Mg (355.0-T6) Solution and Precipitation Heat Treated
  • 1989 SAE AMS4281E-1989 Aluminum Alloy Castings@ Permanent Mold 5.0Si - 1.2Cu - 0.50Mg (355.0- T6) Solution and Precipitation Heat Treated
  • 1978 SAE AMS4281D-1978 ALUMINUM ALLOY CASTINGS@ PERMANENT MOLD 5.0Si - 1.2Cu - 0.50Mg (355.0-T6) (UNS A03550)
  • 1959 SAE AMS4281C-1959 ALUMINUM ALLOY CASTINGS@ PERMANENT MOLD 5Si - 1.2Cu - 0.5Mg (355-T6)
  • 1954 SAE AMS4281B-1954 ALUMINUM ALLOY CASTINGS PERMANENT MOLD 5Si - 1.2Cu - 0.5Mg (355-T6) Solution and Precipitation Treated
  • 1951 SAE AMS4281A-1951 ALUMINUM ALLOY CASTINGS PERMANENT MOLD 5Si - 1.2Cu - 0.5Mg (355-T6) Solution and Precipitation Treated
  • 1945 SAE AMS4281-1945 ALUMINUM ALLOY CASTINGS Permanent Mold 5 Silicon Solution and Precipitation (355-T6)



Copyright ©2024 All Rights Reserved