SAE AMS5390D-1995
Nickel Alloy, Corrosion and Heat Resistant, Investment Castings, 47.5Ni 22Cr 1.5Co 9Mo 0.6W 18.5Fe, As Cast (Reaffirmed: 01 Sept 2000)

Standard No.
SAE AMS5390D-1995
Release Date
1995
Published By
Society of Automotive Engineers (SAE)
Status
 2005-01
Replace By
SAE AMS5390D-2000
Latest
SAE AMS5390G-2019
Scope
This specification covers a corrosion and heat resistant nickel alloy in the form of investment castings. These castings have been used typically for parts, such as turbine vanes and turbine shroud segments, requiring oxidation resistance up to 2200 degrees F (1204 degrees C) and relatively high strength up to 1500 degrees F (816 degrees C), but usage is not limited to such applications.

SAE AMS5390D-1995 history

  • 2019 SAE AMS5390G-2019 Nickel Alloy, Corrosion and Heat-Resistant, Investment Castings 47.5Ni - 22Cr - 1.5Co - 9Mo - 0.60W - 18.5Fe (N-12MV) As-Cast
  • 2014 SAE AMS5390G-2014 Nickel Alloy, Corrosion and Heat Resistant, Investment Castings, 47.5Ni - 22Cr - 1.5Co - 9Mo - 0.6W - 18.5Fe (N-12MV) As-Cast
  • 2013 SAE AMS5390F-2013 Nickel Alloy, Corrosion and Heat Resistant, Investment Castings, 47.5Ni - 22Cr - 1.5Co - 9Mo - 0.6W - 18.5Fe (N-12MV) As-Cast
  • 2011 SAE AMS5390B-2011 ALLOY CASTINGS, INVESTMENT, CORROSION AND HEAT RESISTANT 47.5Ni - 33Cr - 1.5Co - 9Mo - 0.60W - 18.5Fe
  • 2005 SAE AMS5390E-2005 Nickel Alloy, Corrosion and Heat-Resistant, Investment Castings 47.5Ni - 22Cr - 1.5Co - 9Mo - 0.60W - 18.5Fe (N-12MV) As-Cast
  • 2000 SAE AMS5390D-2000 Nickel Alloy, Corrosion and Heat Resistant, Investment Castings 47.5Ni - 22Cr - 1.5Co - 9Mo - 0.60W - 18.5Fe As Cast
  • 1995 SAE AMS5390D-1995 Nickel Alloy, Corrosion and Heat Resistant, Investment Castings, 47.5Ni 22Cr 1.5Co 9Mo 0.6W 18.5Fe, As Cast (Reaffirmed: 01 Sept 2000)
  • 1991 SAE AMS5390C-1991 ALLOY CASTINGS, INVESTMENT, CORROSION AND HEAT RESISTANT 47.5Ni - 22Cr - 1.5Co - 9Mo - 0.60W - 18.5Fe As Cast
  • 1977 SAE AMS5390A-1977 ALLOY CASTINGS, INVESTMENT, CORROSION AND HEAT RESISTANT 47.5Ni - 22Cr - 1.5Co - 9Mo - 0.60W - 18.5Fe
  • 1955 SAE AMS5390-1955 ALLOY CASTINGS, PRECISION INVESTMENT, CORROSION AND HEAT RESISTANT Nickel Base - 22Cr - 1.5Co - 9Mo - 0.6W - 18.5Fe