SAE AMS5843H-2022
Cobalt-Nickel Alloy, Corrosion- and Heat-Resistant, Bars 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb (Nb) - 2.9Ti - 0.20Al - 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated, Work Strengthened, and Aged

Standard No.
SAE AMS5843H-2022
Release Date
2022
Published By
Society of Automotive Engineers (SAE)
Latest
SAE AMS5843H-2022
Scope
This specification covers a high strength, corrosion- and heat-resistant cobalt-nickel-chromium alloy in the form of bars 1-3/4 inches (44.4 mm) and under in nominal diameter.

SAE AMS5843H-2022 history

  • 2022 SAE AMS5843H-2022 Cobalt-Nickel Alloy, Corrosion- and Heat-Resistant, Bars 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb (Nb) - 2.9Ti - 0.20Al - 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated, Work Strengthened, and Aged
  • 2016 SAE AMS5843G-2016 Cobalt-Nickel Alloy@ Corrosion and Heat-Resistant@ Bars 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb (Nb) - 2.9Ti - 0.20Al - 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated@ Work Strengthened@ and Aged (UNS R30159)
  • 2011 SAE AMS5843F-2011 Cobalt-Nickel Alloy, Corrosion and Heat Resistant, Bars 19Cr 36Co 25Ni 7.0Mo 0.50Cb (Nb) 2.9Ti 0.20Al 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted, Solution Heat Treated Work Strengthened and Aged
  • 2006 SAE AMS5843E-2006 Cobalt-Nickel Alloy, Corrosion and Heat Resistant, Bars 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb - 2.9Ti - 0.20Al - 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated, Work Strengthened, and Aged UNS R30159
  • 2000 SAE AMS5843D-2000 Cobalt-Nickel Alloy, Corrosion and Heat Resistant, Bars 19Cr 36Co 25Ni 7.0Mo 0.50Cb 2.9Ti 0.20Al 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted, Solution Heat Treated Work Strengthened and Aged
  • 1995 SAE AMS5843C-1995 Alloy@ Corrosion and Heat Resistant@ Bars 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb - 2.9Ti - 0.20Al - 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated@ Work Strengthened@ and Aged (UNS R30159)
  • 1989 SAE AMS5843B-1989 ALLOY BARS, CORROSION AND HEAT RESISTANT 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb - 2.9Ti - 0.20Al - 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated, Work Strengthened, and Aged
  • 1977 SAE AMS5843-1977 ALLOY BARS, WORK STRENGTHENED, CORROSION AND HEAT RESISTANT 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb - 2.9Ti - 0.20Al - 9.0Fe Solution Heat Treated, Cold Drawn, and Aged
  • 1943 SAE AMS5843A-1943 ALLOY BARS, CORROSION AND HEAT RESISTANT 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb - 2.9Ti - 0.20Al - 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated, Work Strengthened, and Aged
Cobalt-Nickel Alloy, Corrosion- and Heat-Resistant, Bars 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb (Nb) - 2.9Ti - 0.20Al - 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated, Work Strengthened, and Aged



Copyright ©2024 All Rights Reserved