SAE AMS5842B-1988
ALLOY BARS, CORROSION AND HEAT RESISTANT 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb - 2.9Ti - 0.20Al - 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated and Work Strengthened
Home
SAE AMS5842B-1988
Standard No.
SAE AMS5842B-1988
Release Date
1988
Published By
Society of Automotive Engineers (SAE)
Status
Be replaced
1994-01
Replace By
SAE AMS5842C-1994
Latest
SAE AMS5842H-2022
Scope
This specification covers a high strength, corrosion and heat resistant cobalt-chromium-nickel alloy in the form of bars.
SAE AMS5842B-1988 history
2022
SAE AMS5842H-2022
Cobalt-Nickel Alloy, Corrosion- and Heat-Resistant, Bars 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb (Nb) - 2.9Ti - 0.20Al - 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated and Work Strengthened
2016
SAE AMS5842G-2016
Cobalt-Nickel Alloy@ Corrosion and Heat-Resistant@ Bars 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb (Nb) - 2.9Ti - 0.20Al - 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated and Work Strengthened (UNS R30159)
2011
SAE AMS5842F-2011
Cobalt-Nickel Alloy@ Corrosion and Heat-Resistant@ Bars 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb (Nb) - 2.9Ti - 0.20Al - 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated and Work Strengthened (UNS R30159)
2006
SAE AMS5842E-2006
Cobalt-Nickel Alloy, Corrosion and Heat Resistant, Bars 19Cr - 36Co - 25Ni -7.0Mo - 0.50Cb - 2.9Ti - 0.20Al - 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated and Work Strengthened USN R30159
2000
SAE AMS5842D-2000
Cobalt-Nickel Alloy, Corrosion and Heat Resistant, Bars 19Cr 36Co 25Ni 7.0Mo 0.50Cb 2.9Ti 0.20Al 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated and Work Strengthened
1994
SAE AMS5842C-1994
Cobalt-Nickel Alloy@ Corrosion and Heat Resistant@ Bars 19Cr - 36Co - 25Ni -7.0Mo - 0.50Cb - 2.9Ti - 0.20Al - 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated and Work Strengthened (UNS R30159)
1988
SAE AMS5842B-1988
ALLOY BARS, CORROSION AND HEAT RESISTANT 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb - 2.9Ti - 0.20Al - 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated and Work Strengthened
1983
SAE AMS5842A-1983
ALLOY BARS, CORROSION AND HEAT RESISTANT 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb - 2.9Ti - 0.20Al - 9.0Fe Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated and Work Strengthened
1977
SAE AMS5842-1977
ALLOY BARS, WORK STRENGTHENED, CORROSION AND HEAT RESISTANT 19Cr - 36Co - 25Ni - 7.0Mo - 0.50Cb - 2.9Ti - 0.20Al - 9.0Fe Solution Heat Treated and Cold Drawn