SAE AMS5851D-1989
Nickel Alloy, Corrosion and Heat Resistant, Powder 55ni 15cr 17co 5.0mo 3.5ti 4.0al 0.025b, as Fabricated
Home
SAE AMS5851D-1989
Standard No.
SAE AMS5851D-1989
Release Date
1989
Published By
Society of Automotive Engineers (SAE)
Status
Be replaced
1989-01
Replace By
SAE AMS5851C-1994
Latest
SAE AMS5851D-2001
Scope
This specification covers a corrosion and heat resistant nickel alloy in the form of prealloyed powder.
SAE AMS5851D-1989 history
2001
SAE AMS5851D-2001
Nickel Alloy@ Corrosion and Heat Resistant@ Powder 55Ni - 15Cr - 17Co - 5.OMo - 3.5Ti - 4.OAI - 0.025B As Fabricated (UNS N13017)
1994
SAE AMS5851C-1994
Nickel Alloy@ Corrosion and Heat Resistant@ Powder 55Ni - 15Cr - 17Co - 5.0Mo - 4.0A1 - 0.025B as Fabricated (UNS N13017)
1989
SAE AMS5851D-1989
Nickel Alloy, Corrosion and Heat Resistant, Powder 55ni 15cr 17co 5.0mo 3.5ti 4.0al 0.025b, as Fabricated
1989
SAE AMS5851C-1989
Nickel Alloy, Corrosion and Heat Resistant, Powder 55Ni 15Cr 17Co 5.0Mo 3.5Ti 4.0Al 0.025B, As Fabricated (Noncurrent: 01 Apr 1994)
1989
SAE AMS5851B-1989
ALLOY POWDER, CORROSION AND HEAT RESISTANT 55Ni - 15Cr - 17Co - 5.0Mo - 3.5Ti - 4.0Al - 0.025B As Fabricated
1983
SAE AMS5851A-1983
ALLOY POWDER, CORROSION AND HEAT RESISTANT 55Ni - 15Cr - 17Co - 5.0Mo - 3.5Ti - 4.0Al - 0.025B
1977
SAE AMS5851-1977
ALLOY POWDER, CORROSION AND HEAT RESISTANT 55Ni - 15Cr - 17Co - 5.0Mo - 3.5Ti - 4.0Al - 0.025B
Copyright ©2024 All Rights Reserved