SAE AMS5903D-2024
Steel, Corrosion-Resistant, Sheet, Strip, and Plate 18Cr - 9.0Ni (302) Cold Rolled, 1/4 Hard, 125 ksi (862 MPa) Tensile Strength

Standard No.
SAE AMS5903D-2024
Release Date
2024
Published By
Society of Automotive Engineers (SAE)
Latest
SAE AMS5903D-2024
Scope
This specification covers a corrosion-resistant steel in the form of sheet, strip, and plate over 0.005 inch (0.13 mm) in nominal thickness.

SAE AMS5903D-2024 history

  • 2024 SAE AMS5903D-2024 Steel, Corrosion-Resistant, Sheet, Strip, and Plate 18Cr - 9.0Ni (302) Cold Rolled, 1/4 Hard, 125 ksi (862 MPa) Tensile Strength
  • 2018 SAE AMS5903C-2018 Steel@ Corrosion-Resistant@ Sheet@ Strip@ and Plate 18Cr - 9.0Ni (SAE 30302) Cold Rolled@ 1/4 Hard@ 125 ksi (862 MPa) Tensile Strength (UNS S30200)
  • 2012 SAE AMS5903B-2012 Steel, Corrosion-Resistant, Sheet, Strip, and Plate 18Cr - 9.0Ni (SAE 30302) Cold Rolled, 1/4 Hard, 125 ksi (862 MPa) Tensile Strength
  • 2006 SAE AMS5903B-2006 Steel, Corrosion Resistant, Sheet, Strip, and Plate 18Cr - 9.0Ni (SAE 30302) Cold Rolled, 1/4 Hard, 125 ksi (862 MPa) Tensile Strength UNS S30200
  • 2000 SAE AMS5903A-2000 Steel, Corrosion Resistant, Sheet, Strip, and Plate 18Cr 9.0Ni (SAE 30302) Cold Rolled, 1/4 Hard, 125 ksi (862 MPa) Tensile Strength
  • 2000 SAE AMS5903-2000 STEEL SHEET, STRIP, AND PLATE, CORROSION RESISTANT 18Cr - 9.0Ni (SAE 30302) Cold Rolled, 125 ksi (862 MPa) Tensile Strength
  • 1992 SAE AMS5903-1992 Steel Sheet@ Strip@ and Plate@ Corrosion Resistant 18Cr - 9.0Ni (SAE 30302) Cold Rolled@ 125 ksi (862 MPa) Tensile Strength (UNS S30200)