SAE AMS5662-1965
ALLOY BARS@ FORGINGS@ AND RINGS@ CORROSION AND HEAT RESISTANT Nickel Base - 19Cr - 3.1Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al Consumable Electrode or Vacuum Induction Melted@ Solution Treated

Standard No.
SAE AMS5662-1965
Release Date
1965
Published By
SAE - SAE International
Status
 2009-12
Replace By
SAE AMS5662A-1966
Latest
SAE AMS5662P-2022
Scope
APPLICATION: Primarily for parts@ such as flanges@ cases@ and fasteners@ requiring high resistance to creep and stress-rupture up to 1300 F (704 C) and oxidation resistance up to 1800 F (982 C)@ particularly those which are formed or welded and then heat treated to develop required properties.

SAE AMS5662-1965 history

  • 1970 SAE AMS5662P-2022 ALLOY BARS@ FORGINGS@ AND RINGS@ CORROSION AND HEAT RESISTANT Nickel Base - 19Cr - 3.1Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al Consumable Electrode or Vacuum Induction Melted@ Solution Treated
  • 1970 SAE AMS5662N-2016 ALLOY BARS@ FORGINGS@ AND RINGS@ CORROSION AND HEAT RESISTANT Nickel Base - 19Cr - 3.1Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al Consumable Electrode or Vacuum Induction Melted@ Solution Treated
  • 2009 SAE AMS5662M-2009 Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1775 °F (968 °C) Solution Heat Treated, Precipitation-Hardenable
  • 2004 SAE AMS5662M-2004 Nickel Alloy, Corrosion and Heat Resistant, Bars, Forgings, and Rings 52.5Ni 19Cr 3.0Mo 5.1Cb (Nb) 0.90Ti 0.50Al 18Fe, Consumable Electrode or Vacuum Induction Melted 1775°F (968°C) Solution Heat Treated, Precipitation Hardenable
  • 2004 SAE AMS5662E-2004 Nickel Alloy@ Corrosion and Heat-Resistant@ Bars@ Forgings@ and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50AI - 18Fe Consumable Electrode or Vacuum Induction Melted 1775 Degree F (968 Degree C) Solution Heat Treated@ Precipitation-Hardenable
  • 2004 SAE AMS5662B-2004 Nickel Alloy@ Corrosion and Heat-Resistant@ Bars@ Forgings@ and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50AI - 18Fe Consumable Electrode or Vacuum Induction Melted 1775 Degree F (968 Degree C) Solution Heat Treated@ Precipitation-Hardenable
  • 2000 SAE AMS5662L-2000 Nickel Alloy, Corrosion and Heat Resistant, Bars, Forgings, and Rings 52.5Ni 19Cr 3.0Mo 5.1Cb 0.90Ti 0.50Al 18Fe, Consumable Electrode or Vacuum Induction Melted 1775°F (968°C) Solution Heat Treated, Precipitation Hardenable
  • 2000 SAE AMS5662K-2000 Nickel Alloy, Corrosion and Heat Resistant, Bars, Forgings, and Rings 52.5Ni 19Cr 3.0Mo 5.1Cb 0.90Ti 0.50Al 18Fe, Consumable Electrode or Vacuum Induction Melted 1775\mDF (968\mDC) Solution Heat Treated, Precipitation Hardenable
  • 1998 SAE AMS5662K-1998 Nickel Alloy@ Corrosion and Heat Resistant@ Bars@ Forgings@ and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1775 Degrees F (968 Degrees C) Solution Heat Treated@ Precipitation Hardenable (UN
  • 1994 SAE AMS5662J-1994 Nickel Alloy@ Corrosion and Heat Resistant@ Bars@ Forgings@ and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1775 Degrees F (968 Degrees C) Solution Heat Treated@ Precipitation Hardenable (UN
  • 1994 SAE AMS5662H-1994 NICKEL ALLOY@ CORROSION AND HEAT RESISTANT@ BARS@ FORGINGS@ AND RINGS 52.5Ni - 19Cr - 3.0Mo - 5.1Cb - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1775 °F (968 °C) Solution Heat Treated@ Precipitation Hardenable (UNS N07718)
  • 1993 SAE AMS5662G-1993 NICKEL ALLOY@ CORROSION AND HEAT RESISTANT@ BARS@ FORGINGS@ AND RINGS 52.5Ni - 19Cr - 3.0Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1775 °F (968 °C) Solution Heat Treated@ Precipitation Hardenable (UNS N0771
  • 1989 SAE AMS5662F-1989 ALLOY BARS@ FORGINGS@ AND RINGS@ CORROSION AND HEAT RESISTANT 52.5Ni - 19Cr - 3.0Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1775 °F (968 °C) Solution Heat Treated (UNS N07718)
  • 1985 SAE AMS5662E-1985 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT 52.5Ni - 19Cr - 3.0Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1775°F (970°C) Solution Heat Treated
  • 1979 SAE AMS5662D-1979 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT 52.5Ni - 19Cr - 3.0Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1775° F (970° C) Solution Heat Treated
  • 1972 SAE AMS5662C-1972 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19Cr - 3.1Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al - 19Fe Consumable Electrode or Vacuum Induction Melted 1750 F (954.4 C) Solution Heat Treated
  • 1967 SAE AMS5662B-1967 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 19Cr - 3.1Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al Consumable Electrode or Vacuum Induction Melted 1750 F (954.4 C) Solution Heat Treated
  • 1966 SAE AMS5662A-1966 ALLOY BARS@ FORGINGS@ AND RINGS@ CORROSION AND HEAT RESISTANT Nickel Base - 19Cr - 3.1Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al Consumable Electrode or Vacuum Induction Melted@ Solution Treated
  • 1965 SAE AMS5662-1965 ALLOY BARS@ FORGINGS@ AND RINGS@ CORROSION AND HEAT RESISTANT Nickel Base - 19Cr - 3.1Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al Consumable Electrode or Vacuum Induction Melted@ Solution Treated



Copyright ©2024 All Rights Reserved