SAE AMS5590-1966
ALLOY TUBING, SEAMLESS, CORROSION AND HEAT RESISTANT Nickel Base - 19Cr - 3.1Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al Consumable Electrode or Vacuum Induction Melted 1950 F (1065.6 C) Solution Treated

Standard No.
SAE AMS5590-1966
Release Date
1966
Published By
Society of Automotive Engineers (SAE)
Status
Replace By
SAE AMS5590A-1981
Latest
SAE AMS5590G-2023

SAE AMS5590-1966 history

  • 2023 SAE AMS5590G-2023 Nickel Alloy, Corrosion- and Heat-Resistant, Seamless Tubing 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1950 °F (1066 °C) Solution Heat Treated
  • 2018 SAE AMS5590G-2018 Nickel Alloy@ Corrosion and Heat-Resistant@ Seamless Tubing 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1950 °F (1066 °C) Solution Heat Treated (UNS N07718)
  • 2010 SAE AMS5590F-2010 Nickel Alloy@ Corrosion and Heat-Resistant@ Seamless Tubing 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1950 Degree F (1066 Degrees C) Solution Heat Treated (UNS N07718)
  • 2006 SAE AMS5590E-2006 Nickel Alloy, Corrosion and Heat Resistant, Seamless Tubing 52.5Ni - 19Cr - 3.0Mo - 5.1Cb - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1950 °F (1066 °C) Solution Heat Treated
  • 2000 SAE AMS5590E-2000 Nickel Alloy, Corrosion and Heat Resistant, Seamless Tubing 52.5Ni 19Cr 3.0Mo 5.1Cb 0.90Ti 0.50Al 18Fe Consumable Electrode or Vacuum Induction Melted 1950°F (1066°C) Solution Heat Treated
  • 1995 SAE AMS5590D-1995 Nickel Alloy@ Corrosion and Heat Resistant@ Seamless Tubing 52.5Ni - 19Cr - 3.0Mo - 5.1Cb - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1950 Degrees F (1066 Degrees C) Solution Heat Treated (UNS N07718)
  • 1993 SAE AMS5590C-1993 NICKEL ALLOY, CORROSION AND HEAT RESISTANT, SEAMLESS TUBING 52.5Ni - 19Cr - 3.0Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1950 °F (1066 °C) Solution Heat Treated
  • 1991 SAE AMS5590B-1991 ALLOY TUBING, SEAMLESS, CORROSION AND HEAT RESISTANT 52.5Ni - 19Cr - 3.0Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1950°F (1065°C) Solution Heat Treated
  • 1981 SAE AMS5590A-1981 ALLOY TUBING, SEAMLESS, CORROSION AND HEAT RESISTANT 52.5Ni - 19Cr - 3.0Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1950°F (1065°C) Solution Heat Treated
  • 1966 SAE AMS5590-1966 ALLOY TUBING, SEAMLESS, CORROSION AND HEAT RESISTANT Nickel Base - 19Cr - 3.1Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al Consumable Electrode or Vacuum Induction Melted 1950 F (1065.6 C) Solution Treated