SAE AMS4871D-1992
ALUMINUM BRONZE CASTINGS, CENTRIFUGAL AND CHILL 85Cu - 11Al - 3.6Fe Solution Heat Treated and Tempered

Standard No.
SAE AMS4871D-1992
Release Date
1992
Published By
Society of Automotive Engineers (SAE)
Status
 1993-01
Replace By
SAE AMS4871E-1993
Latest
SAE AMS4871H-2015
Scope
This specification covers one type of aluminum bronze in the form of centrifugal and chill castings.

SAE AMS4871D-1992 history

  • 2015 SAE AMS4871H-2015 Aluminum Bronze@ Centrifugal and Chill Castings 85Cu - 11Al - 3.6Fe Solution Heat Treated and Tempered (UNS C95420)
  • 2010 SAE AMS4871G-2010 Aluminum Bronze, Centrifugal and Chill Castings 85Cu 11Al 3.6Fe Solution Heat Treated and Tempered
  • 2006 SAE AMS4871F-2006 Aluminum Bronze, Centrifugal and Chill Castings 85Cu - 11Al - 3.6Fe Solution Heat Treated and Tempered
  • 2000 SAE AMS4871F-2000 Aluminum Bronze, Centrifugal and Chill Castings 85Cu 11Al 3.6Fe Solution Heat Treated and Tempered
  • 1993 SAE AMS4871E-1993 Aluminum Bronze@ Centrifugal and Chill Castings 85Cu - 11Al - 3.6Fe Solution Heat Treated and Tempered (UNS C95420)
  • 1992 SAE AMS4871D-1992 ALUMINUM BRONZE CASTINGS, CENTRIFUGAL AND CHILL 85Cu - 11Al - 3.6Fe Solution Heat Treated and Tempered
  • 1987 SAE AMS4871D-1987 ALUMINUM BRONZE CASTINGS@ CENTRIFUGAL AND CHILL 85Cu - 11Al - 3.6Fe Solution Heat Treated and Tempered (UNS C95420)
  • 1979 SAE AMS4871C-1979 ALUMINUM BRONZE CASTINGS@ CENTRIFUGAL AND CHILL 85Cu - 11Al - 3.6Fe Heat Treated
  • 1951 SAE AMS4871B-1951 ALUMINUM BRONZE CASTINGS@ CENTRIFUGAL AND CHILL 85.3Cu - 10.9Al - 3.6Fe Heat Treated
  • 1946 SAE AMS4871A-1946 Aluminum Bronze Castings Centrifugal or Chill Heat Treated
  • 1942 SAE AMS4871-1942 Aluminum Bronze Castings Heat Treated