SAE AMS6304K-2007
Low-Alloy Steel@ Heat-Resistant@ Bars@ Forgings@ and Tubing 0.95Cr - 0.55Mo - 0.30V (0.40 - 0.50C) (UNS K14675)

Standard No.
SAE AMS6304K-2007
Release Date
2007
Published By
SAE - SAE International
Status
Replace By
SAE AMS6304L-2012
Latest
SAE AMS6304N-2021
Scope
Form: This specification covers an aircraft-quality@ low-alloy@ heat-resistant steel in the form of bars@ forgings@ mechanical tubing@ and forging stock. Application: These products have been used typically for parts@ such as shafts and fasteners@ in service up to 1000 ??(540 ??@ but usage is not limited to such applications.

SAE AMS6304K-2007 history

  • 2021 SAE AMS6304N-2021 Low-Alloy Steel, Heat-Resistant, Bars, Forgings, Mechanical Tubing, and Forging Stock 0.95Cr - 0.55Mo - 0.30V (0.40 - 0.50C)
  • 2016 SAE AMS6304M-2016 Low-Alloy Steel@ Heat-Resistant@ Bars@ Forgings@ and Tubing 0.95Cr - 0.55Mo - 0.30V (0.40 - 0.50C) (UNS K14675)
  • 2012 SAE AMS6304L-2012 Low-Alloy Steel, Heat-Resistant, Bars, Forgings, and Tubing 0.95Cr 0.55Mo 0.30V (0.40-0.50C)
  • 2007 SAE AMS6304K-2007 Low-Alloy Steel@ Heat-Resistant@ Bars@ Forgings@ and Tubing 0.95Cr - 0.55Mo - 0.30V (0.40 - 0.50C) (UNS K14675)
  • 2004 SAE AMS6304J-2004 Low-Alloy Steel, Heat-Resistant, Bars, Forgings, and Tubing 0.95Cr 0.55Mo 0.30V (0.40-0.50C)
  • 2000 SAE AMS6304H-2000 Low-Alloy Steel, Heat-Resistant, Bars, Forgings, and Tubing 0.95Cr - 0.55Mo - 0.30V (0.40 - 0.50C)
  • 1994 SAE AMS6304H-1994 Low-Alloy Steel@ Heat- Resistant@ Bars@ Forgings@ and Tubing 0.95Cr - 0.55Mo - 0.30V (0.40 - 0.50C) (UNS K14675)