SAE AMS4223B-1989
Aluminum Alloy Castings 4.5Cu - 0.70Ag - 0.30Mn - 0.25Mg - 0.25Ti (A201.0-T4) Solution Heat Treated and Naturally Aged (UNS A12010)

Standard No.
SAE AMS4223B-1989
Release Date
1989
Published By
SAE - SAE International
Status
Replace By
SAE AMS4223B-1995
Latest
SAE AMS4223E-2015
Scope
Form: This specification covers an aluminum alloy in the form of sand@ permanent mold@ and composite mold casings. Application: Primarily for components requiring high strength combined with good ductility and impact strength. Certain design and processing procedures may cause these castings to become susceptible to stress-corrosion cracking.

SAE AMS4223B-1989 history

  • 2015 SAE AMS4223E-2015 Aluminum Alloy@ Castings 4.5Cu - 0.70Ag - 0.30Mn - 0.25Mg - 0.25Ti (A201.0-T4) Solution Heat Treated and Naturally Aged (UNS A12010)
  • 2012 SAE AMS4223D-2012 Aluminum Alloy, Castings 4.5Cu - 0.70Ag - 0.30Mn - 0.25Mg - 0.25Ti (A201.0-T4) Solution Heat Treated and Naturally Aged
  • 2007 SAE AMS4223D-2007 Aluminum Alloy, Castings 4.5Cu - 0.70Ag - 0.30Mn - 0.25Mg - 0.25Ti (A201.0-T4) Solution Heat Treated and Naturally Aged
  • 1996 SAE AMS4223C-1996 Aluminum Alloy, Castings 4.5Cu 0.70Ag 0.30Mn 0.25Mg 0.25Ti, Solution Heat Treated and Naturally Aged
  • 1995 SAE AMS4223B-1995 ALUMINUM ALLOY CASTINGS 4.5Cu - 0.70Ag - 0.30Mn - 0.25Mg - 0.25Ti (A201.0-T4) Solution Heat Treated and Naturally Aged
  • 1989 SAE AMS4223B-1989 Aluminum Alloy Castings 4.5Cu - 0.70Ag - 0.30Mn - 0.25Mg - 0.25Ti (A201.0-T4) Solution Heat Treated and Naturally Aged (UNS A12010)
  • 1982 SAE AMS4223A-1982 Aluminum Alloy Castings 4.5Cu - 0.70Ag - 0.30Mn - 0.25Mg - 0.25Ti (A201.0-T4) Solution Heat Treated and Naturally Aged (UNS A12010)
  • 1974 SAE AMS4223-1974 ALUMINUM ALLOY CASTINGS 4.5Cu - 0.70Ag - 0.30Mn - 0.25Mg - 0.25Ti (A201.0-T4) Solution Heat Treated and Naturally Aged