PREN 3499-1988
Titanium TI-P04 Annealed 570 Less Than or Equal to Rm Less Than or Equal to 730 MPa Sheet and Strip@ Cold Rolled A Less Than or Equal to 3 mm

Standard No.
PREN 3499-1988
Release Date
1988
Published By
ASD-STAN - Aerospace and Defence Industries Association of Europe - Standardization
Status
 1997-08
Replace By
PREN 3499-1993
Latest
PREN 3499-1993

PREN 3499-1988 history

  • 1993 PREN 3499-1993 Aerospace Series Titanium TI-P99003 Annealed Sheet and Strip@ Cold Rolled a Less Than or Equal to 6 mm 570 MPa Less Than or Equal to Rm Less Than or Equal to 730 MPa (Edition P 2)
  • 1988 PREN 3499-1988 Titanium TI-P04 Annealed 570 Less Than or Equal to Rm Less Than or Equal to 730 MPa Sheet and Strip@ Cold Rolled A Less Than or Equal to 3 mm