SAE AMS5583C-1995
Nickel Alloy@ Corrosion and Heat Resistant@ Seamless Tubing 72Ni - 15.5Cr - 0.95Cb - 2.5Ti - 0.70Al - 7.0Fe Solution Heat Treated (UNS N07750)

Standard No.
SAE AMS5583C-1995
Release Date
1995
Published By
SAE - SAE International
Status
Replace By
SAE AMS5583D-2002
Latest
SAE AMS5583F-2019

SAE AMS5583C-1995 history

  • 2019 SAE AMS5583F-2019 Nickel Alloy@ Corrosion and Heat-Resistant@ Seamless Tubing 72Ni - 15.5Cr - 0.95Cb (Nb) - 2.5Ti - 0.70Al - 7.0Fe Vacuum Melted Solution Heat Treated@ Precipitation Hardenable to 170 ksi (1172 MPa) Tensile Strength (UNS N07750)
  • 2013 SAE AMS5583E-2013 Nickel Alloy, Corrosion and Heat Resistant, Seamless Tubing 72Ni 15.5Cr 0.95Cb (Nb) 2.5Ti 0.70Al 7.0Fe, Vacuum Melted Solution Heat Treated, Precipitation Hardenable to 170 ksi (1172 MPa) Tensile Strength
  • 2011 SAE AMS5583B-2011 ALLOY TUBING, SEAMLESS, CORROSION AND HEAT RESISTANT 72Ni - 15.5Cr - 0.95(Cb + Ta) - 2.6Ti - 0.70Al - 7.0Fe Solution Heat Treated
  • 2006 SAE AMS5583D-2006 Nickel Alloy, Corrosion and Heat-Resistant, Seamless Tubing 72Ni - 15.5Cr - 0.95Cb - 2.5Ti - 0.70Al - 7.0Fe Vacuum Melted Solution Heat Treated, Precipitation Hardenable to 170 ksi (1172 MPa) Tensile Strength
  • 2002 SAE AMS5583D-2002 Nickel Alloy, Corrosion and Heat-Resistant, Seamless Tubing 72Ni - 15.5Cr - 0.95Cb - 2.5Ti - 0.70Al - 7.0Fe Vacuum Melted Solution Heat Treated, Precipitation Hardenable to 170 ksi (1172 MPa) Tensile Strength UNS N07750
  • 1995 SAE AMS5583C-1995 Nickel Alloy@ Corrosion and Heat Resistant@ Seamless Tubing 72Ni - 15.5Cr - 0.95Cb - 2.5Ti - 0.70Al - 7.0Fe Solution Heat Treated (UNS N07750)
  • 1984 SAE AMS5583A-1984 ALLOY TUBING, SEAMLESS, CORROSION AND HEAT RESISTANT 72Ni - 15.5Cr - 0.95(Cb + Ta) - 2.6Ti - 0.70Al - 7.0Fe Solution Heat Treated
  • 1977 SAE AMS5583-1977 ALLOY TUBING, SEAMLESS, CORROSION AND HEAT RESISTANT 72Ni - 15.5Cr - 0.95(Cb+Ta) - 2.6Ti - 0.70Al - 7.0Fe Premium Quality