SAE AMS5870G-2024
Nickel Alloy, Corrosion- and Heat-Resistant, Sheet, Strip, and Plate 60.5Ni - 23Cr - 14Fe - 0.35Ti - 1.4Al (Alloy 601), Solution Heat Treated
Home
SAE AMS5870G-2024
Standard No.
SAE AMS5870G-2024
Release Date
2024
Published By
Society of Automotive Engineers (SAE)
Latest
SAE AMS5870G-2024
Scope
This specification covers a corrosion- and heat-resistant nickel alloy in the form of sheet, strip, and plate 0.010 to 2.000 inches (0.25 to 50.80 mm), inclusive, in nominal thickness.
SAE AMS5870G-2024 history
2024
SAE AMS5870G-2024
Nickel Alloy, Corrosion- and Heat-Resistant, Sheet, Strip, and Plate 60.5Ni - 23Cr - 14Fe - 0.35Ti - 1.4Al (Alloy 601), Solution Heat Treated
2019
SAE AMS5870F-2019
Nickel Alloy@ Corrosion and Heat-Resistant@ Sheet@ Strip@ and Plate 60.5Ni - 23Cr - 14Fe - 0.35Ti - 1.4Al Solution Heat Treated (UNS N06601)
2012
SAE AMS5870E-2012
Nickel Alloy, Corrosion and Heat Resistant, Sheet, Strip and Plate 60.5Ni 23Cr 14Fe 0.35Ti 1.4Al Solution Heat Treated
2011
SAE AMS5870B-2011
ALLOY SHEET, STRIP, AND PLATE, CORROSION AND HEAT RESISTANT 60.5Ni - 23Cr - 14Fe - 0.35Ti - 1.4Al Solution Heat Treated
2006
SAE AMS5870D-2006
Nickel Alloy, Corrosion and Heat Resistant, Sheet, Strip, and Plate 60.5Ni - 23Cr - 14Fe - 0.35Ti - 1.4Al Solution Heat Treated UNS N06601
2000
SAE AMS5870C-2000
Nickel Alloy, Corrosion and Heat Resistant, Sheet, Strip, and Plate 60.5Ni - 23Cr - 14Fe - 0.35Ti - 1.4Al Solution Heat Treated
1993
SAE AMS5870C-1993
Nickel Alloy, Corrosion and Heat Resistant, Sheet, Strip and Plate 60.5Ni 23Cr 14Fe 0.35Ti 1.4Al Solution Heat Treated
1979
SAE AMS5870A-1979
ALLOY SHEET, STRIP, AND PLATE, CORROSION AND HEAT RESISTANT 60.5Ni - 23Cr - 14Fe - 1.4Al
1972
SAE AMS5870-1972
ALLOY SHEET, STRIP, AND PLATE, CORROSION AND HEAT RESISTANT Nickel Base - 23Cr - 14Fe - 1.35Al
Copyright ©2024 All Rights Reserved