SAE AMS5363D-1987
Steel Castings@ Sand and Centrifugal@ Corrosion and Heat Resistant 18.5Cr - 10.5Ni - 0.90 (Cb+Ta) Solution Heat Treated (UNS J92641)

Standard No.
SAE AMS5363D-1987
Release Date
1987
Published By
SAE - SAE International
Status
Replace By
SAE AMS5363E-1995
Latest
SAE AMS5363F-2017
Scope
Form: This specification covers a corrosion and heat resistant steel in the orri of sand or centrifugal castings. Application: Primarily for parts requiring corrosion and heat resistance up to 80C??(425??@ especially when such parts are welded during fabrication@ and for parts requiring oxidation resistance up to 1500??(815?? but useful at that temperature only when stresses are low.

SAE AMS5363D-1987 history

  • 2017 SAE AMS5363F-2017 Steel Castings@ Sand and Centrifugal@ Corrosion and Heat Resistant 18.5Cr - 10.5Ni - 0.90 (Cb+Ta) Solution Heat Treated (UNS J92641)
  • 2012 SAE AMS5363E-2012 Steel Castings, Sand and Centrifugal, Corrosion and Heat Resistant 18.5Cr - 10.5Ni - 0.90 (Cb+Ta) Solution Heat Treated
  • 2011 SAE AMS5363D-2011 STEEL CASTINGS, SAND AND CENTRIFUGAL, CORROSION AND HEAT RESISTANT 18.5Cr - 10.5Ni - 0.90(Cb+Ta) Solution Heat Treated
  • 1995 SAE AMS5363E-1995 Steel Castings, Sand and Centrifugal, Corrosion and Heat Resistant 18.5Cr - 10.5Ni - 0.90 (Cb+Ta) Solution Heat Treated UNS J92641; R (2002)
  • 1987 SAE AMS5363D-1987 Steel Castings@ Sand and Centrifugal@ Corrosion and Heat Resistant 18.5Cr - 10.5Ni - 0.90 (Cb+Ta) Solution Heat Treated (UNS J92641)
  • 1978 SAE AMS5363C-1978 STEEL CASTINGS, SAND AND CENTRIFUGAL, CORROSION AND HEAT RESISTANT 18.5Cr - 10.5Ni - 0.90(Cb+Ta)
  • 1958 SAE AMS5363B-1958 STEEL CASTINGS, SAND AND CENTRIFUGAL, CORROSION AND HEAT RESISTANT 18Cr - 10.5Ni - (Cb+Ta)
  • 1950 SAE AMS5363A-1950 STEEL CASTINGS, SAND, CORROSION AND HEAT RESISTANT 18Cr - 10.5Ni - (Cb+Ta)
  • 1947 SAE AMS5363-1947 STEEL CASTINGS, SAND, CORROSION AND HEAT RESISTANT 18Cr - 10.5Ni - Cb