SAE AMS5750C-2012
Alloy Bars, Forgings, and Rings, Corrosion and Heat Resistant Nickel Base - 15.5Cr - 16Mo - 3.8W - 5.5Fe Solution Heat Treated

Standard No.
SAE AMS5750C-2012
Release Date
2012
Published By
Society of Automotive Engineers (SAE)
Status
 2017-04
Replace By
SAE AMS5750D-2017
Latest
SAE AMS5750D-2017
Scope
This specification covers a corrosion and heat resistant nickel-base alloy in the form of bars, forgings, flash welded rings, and stock for forging or flash welded rings.

SAE AMS5750C-2012 history

  • 2017 SAE AMS5750D-2017 Alloy Bars@ Forgings@ and Rings@ Corrosion and Heat Resistant Nickel Base - 15.5Cr - 16Mo - 3.8W - 5.5Fe Solution Heat Treated
  • 2012 SAE AMS5750C-2012 Alloy Bars, Forgings, and Rings, Corrosion and Heat Resistant Nickel Base - 15.5Cr - 16Mo - 3.8W - 5.5Fe Solution Heat Treated
  • 1991 SAE AMS5750B-1991 ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT Nickel Base - 15.5Cr - 16Mo - 3.8W - 5.5Fe Solution Heat Treated
  • 1980 SAE AMS5750C-1980 (Noncurrent)Alloy Bars, Forgings, and Rings, Corrosion and Heat Resistant Nickel Base - 15.5Cr - 16Mo - 3.8W - 5.5Fe Solution Heat Treated R(2000)
  • 1964 SAE AMS5750A-1964 ALLOY BARS, FORGINGS, AND RINGS, CORROSION & HEAT RESISTANT Nickel Base - 15.5Cr - 16Mo - 4W - 6Fe Solution Treated
  • 1953 SAE AMS5750-1953 ALLOY, CORROSION AND HEAT RESISTANT Nickel Base - 16Mo - 15.5Cr - 6Fe - 4W