SAE AMS5881-1975
ALLOY FORGINGS, CORROSION AND HEAT RESISTANT 59.5Ni - 12Cr - 10Co - 3.0Mo - 6.0W - 3.0Ti - 1.5Ta - 4.5Al - 0.015B - 0.10Zr (0.30 - 0.35C) Solution, Stabilized, and Precipitation Heat Treated

Standard No.
SAE AMS5881-1975
Release Date
1975
Published By
Society of Automotive Engineers (SAE)
Status
 2004-07
Replace By
SAE AMS5881B-1993
Latest
SAE AMS5881A-2011
Scope
This specification covers a corrosion and heat resistant nickel alloy powder-metallurgy product in the form of forgings.

SAE AMS5881-1975 history

  • 2011 SAE AMS5881A-2011 ALLOY FORGINGS, CORROSION AND HEAT RESISTANT 59.5Ni - 12Cr - 10Co - 3.0Mo - 6.0W - 3.0Ti - 1.5Ta - 4.5Al - 0.015B - 0.10Zr (0.30 - 0.35C), Solution, Stabilized, and Precipitation Heat Treated
  • 1993 SAE AMS5881B-1993 ALLOY FORGINGS@ CORROSION AND HEAT RESISTANT 59.5NI - 12CR - 10CO - 3.0MO - 6.0W - 3.0TI - 1.5TA - 4.5A1 - 0.15B - 0.10ZR (0.30 - 0.35C)@ SOLUTION@ STABILIZED@ AND PRECIPITATION HEAT TREATED
  • 1975 SAE AMS5881-1975 ALLOY FORGINGS, CORROSION AND HEAT RESISTANT 59.5Ni - 12Cr - 10Co - 3.0Mo - 6.0W - 3.0Ti - 1.5Ta - 4.5Al - 0.015B - 0.10Zr (0.30 - 0.35C) Solution, Stabilized, and Precipitation Heat Treated



Copyright ©2024 All Rights Reserved