T/CWAN 0103-2024
Scope
This document specifies the model, technical requirements, inspection methods, inspection rules, marking, packaging, transportation and storage of high-temperature alloy laser welding activators. This document applies to activators for laser welding of high temperature alloys. Among them, laser welding includes single laser welding, laser filler wire welding and laser-arc hybrid welding.
T/CWAN 0103-2024 history
2024T/CWAN 0103-2024 Active agents for laser welding of superalloy