ISO/DIS 18177:2024
Plastics — Test method for estimation of the short chain branching distribution of semicrystalline ethylene 1-olefin copolymers by differential scanning calorimetry (DSC)

Standard No.
ISO/DIS 18177:2024
Release Date
2024
Published By
International Organization for Standardization (ISO)  IX  /  ISO
Latest
ISO/DIS 18177:2024
 

Introduction
This document outlines a method for determining the distribution of short-chain branching in semi-crystalline ethylene-α-olefin copolymers using differential scanning calorimetry (DSC). The technique described is applicable to various types of ethylene-α-olefin copolymers and provides guidance on sample preparation, measurement conditions, data analysis, and reporting results. It aims to offer consistent and reliable methods for assessing the short-chain branching distribution in these materials.

ISO/DIS 18177:2024 history

  • 2024 ISO/DIS 18177:2024 Plastics — Test method for estimation of the short chain branching distribution of semicrystalline ethylene 1-olefin copolymers by differential scanning calorimetry (DSC)

Topics on standards and specifications

Standard and Specification

24/30463784 DC Plastics - Test method for estimation of the short chain branching distribution of semicrystalline ethylene 1-olefin copolymers by differential scanning calorimetry (DSC) ISO 18177:2025 PlasticsTest method for estimation of the short chain branching distribution of semicrystalline ethylene 1-olefin copolymersDifferential scanning calorimetry (DSC) BS ISO 18177:2025 Plastics. Test method for estimation of the short chain branching distribution of semicrystalline ethylene 1-olefin copolymers. Differential scanning calorimetry (DSC) UNI ISO 18177:2025 PlasticsTest method for estimation of the short chain branching distribution of semicrystalline ethylene 1-olefin copolymersDifferential scanning calorimetry (DSC) BS EN 62788-1-6:2017+A1:2020 Measurement procedures for materials used in photovoltaic modules - Encapsulants. Test methods for determining the degree of cure in Ethylene-Vinyl Acetate ANSI/ASTM D4591:2001 Test Method for Determining Temperatures and Heats of Transitions of Fluoropolymers by Differential Scanning Calorimetry ASTM D4591-97 Standard Test Method for Determining Temperatures and Heats of Transitions of Fluoropolymers by Differential Scanning Calorimetry ASTM D4591-01 Standard Test Method for Determining Temperatures and Heats of Transitions of Fluoropolymers by Differential Scanning Calorimetry ASTM D5017-96(2003)e1 Standard Test Method for Determination of Linear Low Density Polyethylene (LLDPE) Composition by Carbon-13 Nuclear Magnetic Resonance